Maximum length of 100 characters reached
6022I125, Techniweld Decking Rod 1/8" Diameter
Designed for welding roof decking to support beams and other similar applications where burn-through spot welds with full penetration are required.
Filler Metals Electrode, 10 lb Net Content, Cardboard Container, 1/8 in Diameter, 60000 lb Tensile Strength, Composition: 0.14% Carbon, 0.025% Phosphorus, 0.03% Chromium, 1.2% Manganese, 0.012% Sulfur, 0.01% Molybdenum, 0.28% Silicon, 0.02% Nickel, 80/140 A
| Amperage Rating | : | 80/140 amp |
| Composition | : | 0.14% Carbon, 0.025% Phosphorus, 0.03% Chromium, 1.2% Manganese, 0.012% Sulfur, 0.01% Molybdenum, 0.28% Silicon, 0.02% Nickel |
| Container Type | : | Cardboard |
| Diameter | : | 1/8" |
| Net Content | : | 10 lb |
| Tensile Strength | : | 60,000 lb |